Industry Application Conditions Material
Food Baking Ovens
Char Retort, Sugar
Vegetables and Fruit
400-900 °F
500-700 °F
200-300 °F
Wrought Iron – Bare Thermocouple
Wrought Iron
304 Stainless Steel
Gas Producer gas
Water gas
     carburetor
     superheater
Tar stills
  28% Chrome Iron – Inconel 601

Inconel 600 – 28% Chrome Iron
Inconel 600 – 28% Chrome Iron
C1018 Steel

Glass Melting tank
     roof & wall
     flues and checkers
Forehearth and feeder
Lehr
Open Hearth Roof
to 2400 °F
to 1800 °F
to 2200 °F
300-500 °F
C30 Ceramic
Inconel 600 – 28% Chrome Iron – Wrought Iron
Bare Platinum Thremocouple
Wrought Iron
LT-1
Heat
Treatine
Annealing

Hardening
     open fired or electric heated

     H. S. Tool Steel
     Salt Baths
          Neutral
          High Speed
     Lead Pot
     Cyanide Pot

     Lavite Pot
     Carburizing
          gas
          cyanide pot
     Nitriding
     Quench Oil

to 1200 °F
   1300-2000 °F

to 1500 °F
     to 2000 °F
     to 2400 °F
to 2350 °F

to 2000 °F
to 2350 °F
to 2000 °F
1750 °F
     2350 °F
2400 °F

to 2000 °F

to 1000 °F
900 °F

Wrought Iron
Inconel 600 – Inconel 601 – 28% Chrome Iron (for sulphur atmospheres)

Wrought Iron
Inconel 600 – 28% Chrome Iron
C30 Ceramic
Inconel 600 – Nickel

28% Chrome Iron
C30 Ceramic
28% Chrome Iron
Inconel 600 – Nickel
Nickel
Inconel 600 – 28% Chrome Iron

Inconel 601 – 28% Chrome Iron
Nickel
28% Chrome Iron
Wrought Iron

Iron
and
Steel
Blast Furnace
     down comer
     stove dome
     stock trunk
     stove outlet flue
     hot blast main
Open Hearth
     flues and stack
     checkers
Waste Head Boilers
Soaking Pits

Billet and Slab Furnace

Forging Furnace
Annealing
Bright Annealing
     batch
     continuous
Pickling
Galvanizing
Tinning
     tin pot
     palm oil
Vacuum Melting (Induction Melting)

1800-2300 °F

900-1600 °F

to 1800 °F
to 2200 °F
to 1600 °F
2000 °F
   Over 2000 °F
2000 °F
   Over 2000 °F
2000-2400 °F

to 3200 °F

Inconel 601 – 28% Chrome Iron – Silicon Carbide – Silicon Nitride
Silicon Carbide – Silicon Nitride
Inconel 600
Wrought Iron
Inconel 601 – 28% Chrome Iron

Inconel 601 – 28% Chrome Iron – LT-1
Inconel 601 – LT-1
Inconel 601 – 28% Chrome Iron
Inconel 601 – 28% Chrome Iron – Silicon Carbide – Silicon Nitride
Silicon Carbide – C30 Ceramic – Silicon Nitride
Inconel 601 – 28% Chrome Iron
Silicon Carbide – C30 Ceramic – Silicon Nitride
Silicon Carbide – C30 Ceramic – Silicon Nitride
Inconel 600 – Inconel 601 or 28% Chrome Iron
     (for sulphur atmospheres)
Inconel 600
C30 Ceramic – Silicon Carbide – Silicon Nitride
     Lead Sheath – Silicon Carbide – Silicon Nitride
XH Seamless Steel – Silicon Carbide – Silicon Nitride

Seamless Steel – 28% Chrome Iron – Silicon Carbide – Silicon Nitride
304 Stainless Steel
C98 Ceramic

Non-Ferrous
Metals
Aluminum
     melting pot
     pouring ladles

     furnaces
     heat treating
     die casting
Magnesium
     melt
     die casting
     ladle
Lead
     pots

1300 to 1400 °F

950 °F
800-1300 °F

1000 °F
     1500 °F

Cast Iron (Washed) – Silicon Carbide – Silicon Nitride
Open end thermocouple assemblies

304 Stainless Steel Cerampak
Wrought Iron – 304 Stainless Steel Cerampak
Cast Iron – Wrought Iron – Silicon Carbide

Wrought Iron
Wrought Iron
Wrought Iron

Wrought Iron
28% Chrome Iron – Silicon Carbide – Silicon Nitride

 

< Previous Next >