Industry Application Conditions Material
Nonferrous
Metals
Continued
Brass
     ladle
     billet and forging
     anneal
Copper
     molten
     smelting & ore roasters

Tin
     pot
Zinc
     die casting

500 °F

800 °F

LT-1 – Silicon Carbide – Silicon Nitride – Immersion T/C
Inconel 601 – 28% Chrome Iron
Wrought Iron – 304 Stainless Steel Cerampak

Silicon Nitride- LT-1
Inconel 601 – 28% Chrome Iron – C30 Ceramic – Silicon Carbide – Silicon Nitride

XH Seamless Steel – Silicon Carbide – Silicon Nitride

XH Seamless Steel – Silicon Carbide – Silicon Nitride

Paper Digesters
Sulphur Burners
220-300 °F
900-1400 °F
316 Stainless Steel – Tantalum Sleeved
Inconel 601 – 28% Chrome Iron – LT-1
Petroleum Cracking lines
Dewaxing
Fractionating column top tower
Reaction chamber
Tube still inlet
Tube still bridge wall
950 °F
minus 20 °F
150-500 °F
850-890 °F
575-700 °F
1500-2200 °F
304 Stainless Steel
304 Stainless Steel
304 Stainless Steel
304 Stainless Steel
304 Stainless Steel
Inconel 600
Power
and Heat
Fire Box
Flue gas

Preheaters
Steam lines
Powdered coal air
Diesel engine exhaust
Water lines

1800-2200 °F
450-1000 °F

200-500 °F
300-950 °F
500 °F
600 °F

Inconel 600
304 Stainless Steel Cerampak
     Wrought Iron – 28% Chrome Iron
Wrought Iron – 304 Stainless Steel Cerampak
304 Stainless Steel
304 Stainless Steel
304 Stainless Steel
C1018 Carbon Steel
Smelting
and Refining
Roasting sulphur ores
Zinc retort preheater
Zinc spelter
700-1900 °F
1300-2400 °F
700-900 °F
28% Chrome Iron – Inconel 601
C30 Ceramic
28% Chrome Iron
Misc. Asphalt mixing
Incinerator
to 2000 °F
over 2000 °F
Wrought Iron – Sand Thermocouple
Inconel 601 – 28% Chrome Iron
C30 Ceramic – SiIicon Carbide – SiIicon Nitride

 